MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Spartech Royalite R21M General Purpose ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable tape decks, telephones and office furniture trim.

Key Words: Poly(Acrylonitrile-Butadiene-Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Water Absorption 0.050 %0.050 %24 hrs. ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inASTM D955
Melt Flow 1.7 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.7 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Condition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9898ASTM D785
Tensile Strength, Yield 33.9 MPa4920 psiASTM D638
Modulus of Elasticity 2.10 GPa305 ksiASTM D638
Flexural Yield Strength 59.9 MPa8690 psiASTM D790
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched 4.10 J/cm7.68 ft-lb/inASTM D256
 1.10 J/cm
@Temperature -20.0 °C
2.06 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 139 µm/m-°C
@Temperature 20.0 °C
77.2 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FAnnealed; ASTM D648
Vicat Softening Point 92.0 °C198 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Tabriz HR 2340 Acrylonitrile Butadiene Styrene
Omnia Plastica ABS Acrylonitrile-butadiene-styrene
Mitsubishi Iupilon® LCH 2315 Polycarbonate

PROY34 / 66394

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.