MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient PolyOne® 4474 Ethylene-Propylene Diene Elastomer (EPDM) Compound  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

PolyOne Chemical Cure EPDM wire and cable compounds include a full range of thermoset elastomers ranging from natural rubber to fluoroelastomers. Rubber offers excellent thermal and chemical resistance in a broad range of Durometer (Shore A and D) for applications in the wire and cable industry.

Description/Features:

  • Control cable and instrumentation

Applications:

  • Insulation

Market:

  • Wire & Cable

Note: Tensile Strength and Elongation measured on No. 12 AWG with 1.18mm Wall.
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 11.55 MPa1675 psiType 4 - Flexibles, Break, 20 in/min; ASTM D638
Elongation at Break 290 %290 %Type 4 - Flexibles, 20 in/min; ASTM D638
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
Cold BendNo Cracks, -40°FUL 1581
Mechanical Water Absorption0.00142916962513882oz/in²7 days @ 70ºC, UL 1581
Oven Aged - Retention of Elongation (ROE)200%325°F(163°C), 168 hrs (7 days), 0.075 in, UL Standard
 200%325°F(163°C), 240 hrs (10 days), 0.075 in, UL Standard
 59%302°F(150°C), 720 hrs (30 days), 0.075 in, UL Standard
Oven Aged - Retention of Tensile Strength (ROT)1260%325°F(163°C), 168 hrs (7 days), 0.075 in, UL Standard
 1275%325°F(163°C), 240 hrs (10 days), 0.075 in, UL Standard
 76%302°F(150°C), 720 hrs (30 days), 0.075 in, UL Standard

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Avient PolyOne® ND-10 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
Armacell Monarch® F-03092 (Black) EPDM Foam
E-Polymers EFLEX® V1040 EPDM/TPV

PH1PO3438 / 45077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.