PolyOne Chemical Cure EPDM wire and cable compounds include a full range of thermoset elastomers ranging from natural rubber to fluoroelastomers. Rubber offers excellent thermal and chemical resistance in a broad range of Durometer (Shore A and D) for applications in the wire and cable industry. Description/Features: - Control cable and instrumentation
Applications: Market: Note: Tensile Strength and Elongation measured on No. 12 AWG with 1.18mm Wall. PolyOne First Choice Information provided by PolyOne Corporation. |