Resistat F901, MERGE R055 is a 55-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of approximately 1 micron. The yarn color is black. Resistat is used for carpeting, ESD garments, and industrial belting and brushes. Information provided by Shakespeare Company. |