MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zeus PFA Tubing and Drawn Fiber
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that are SEMI F-57 certified, lending itself to critical fluid transport tubing applications that demand a very low level of extractables. This fluoropolymer can be extruded in convoluted tubing forms that provide a highly flexible conduit.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.12 - 2.17 g/cc0.0766 - 0.0784 lb/in³ASTM D792
Water Absorption <= 0.030 %<= 0.030 %ASTM D257
Crystallinity 48 - 70 %48 - 70 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6055 - 60ASTM D2240
Tensile Strength, Ultimate 25.0 - 35.0 MPa3630 - 5080 psiASTM D638
Elongation at Break 250 - 420 %250 - 420 %ASTM D638
Modulus of Elasticity 0.450 GPa65.3 ksiASTM D638
Flexural Modulus 0.600 - 0.700 GPa87.0 - 102 ksiASTM D790
Coefficient of Friction 0.040 - 0.200.040 - 0.20
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmASTM D257
Dielectric Constant 1.9 - 2.1
@Frequency 1e+6 Hz
1.9 - 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.7 - 78.7 kV/mm500 - 2000 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 - 140 µm/m-°C
@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.150 - 0.250 W/m-K1.04 - 1.74 BTU-in/hr-ft²-°FASTM C177
Melting Point 300 - 315 °C572 - 599 °F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -200 °C-328 °F
Glass Transition Temp, Tg 100 °C212 °F
Decomposition Temperature 475 °C887 °FASTM E1131
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.351.35
 
Descriptive Properties
Radiation Resistance (MRad)1 to 10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zeus FEP Tubing and Drawn Fiber
Mitsubishi Chemical Advanced Materials Techtron™ 1000 PPS Extruded Polyphenylene Sulfide
Overview of materials for Polyetheretherketone, PTFE Filled
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
Daikin NEOFLON® AP-230 PFA

PZEUS993 / 178058

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.