Teflon™ PFA 440HPB is a special purpose fluoroplastic resin available in pellet form. This resin is a chemically modified form of Teflon™ PFA 340 that combines many of the benefits of the parent resin (a relatively high typical melt flow rate of 14) with several additional benefits including enhanced purity, improved thermal stability while processing, and chemical inertness; for example, to ozonated fluids. Applications for Teflon™ PFA 440HPB include fluid handling components for critical, high-purity processes, like semiconductor, pharmaceutical, and biotechnology, as well as applications where purity in the parts-per-billion range is needed. Teflon™ PFA 440HPB offers a slightly lower melt flow rate than Teflon™ PFA 440HPA, ultimately providing a higher degree of stress crack resistance.Information provided by Chemours. |