MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemours Teflon™ PFA 440HPB Special purpose fluoroplastic resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Teflon™ PFA 440HPB is a special purpose fluoroplastic resin available in pellet form. This resin is a chemically modified form of Teflon™ PFA 340 that combines many of the benefits of the parent resin (a relatively high typical melt flow rate of 14) with several additional benefits including enhanced purity, improved thermal stability while processing, and chemical inertness; for example, to ozonated fluids. Applications for Teflon™ PFA 440HPB include fluid handling components for critical, high-purity processes, like semiconductor, pharmaceutical, and biotechnology, as well as applications where purity in the parts-per-billion range is needed. Teflon™ PFA 440HPB offers a slightly lower melt flow rate than Teflon™ PFA 440HPA, ultimately providing a higher degree of stress crack resistance.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.15 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
ASTM D570
Melt Flow 14 g/10 minASTM D3307
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D2240
Tensile Strength 14.0 MPa
@Temperature 250 °C
ASTM D3307
 25.0 MPa
@Temperature 23.0 °C
ASTM D3307
Elongation, Ultimate 300 %
@Temperature 23.0 °C
ASTM D3307
 480 %
@Temperature 250 °C
ASTM D3307
Flexural Modulus 0.0550 GPa
@Temperature 250 °C
ASTM D790
 0.590 GPa
@Temperature 23.0 °C
ASTM D790
Flex Crack Resistance 30000
@Thickness 0.203 mm
Cycles MIT Folding Endurance; ASTM D2176
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohmASTM D257
Dielectric Constant 2.03
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.250 mm
Short Time; ASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 305 °CASTM D4591
Maximum Service Temperature, Air 260 °CContinuous, per accelerated heat-aging test
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Critical Shear Rate (1/s)50372°C
Heat of Combustion5.3 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceOutstanding
Weather Resistance (years unaffected)10Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8804 / 268730

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.