MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Ultrathene UE650028 Ethylene Vinyl Acetate Copolymer (EVA), Blow Molding Grade
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Blow MoldingGrade

Material Notes: Ultrathene UE650028 is an EVA copolymer with excellent flexibility and low temperature properties. Applications: Foamed Sheet, Soft Profile & Sheets

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.931 g/cc0.0336 lb/in³ASTM D1505
Vinyl Acetate Content 12 %12 %LYB Method
Melt Flow 3.0 g/10 min3.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4444ASTM D 2240
Tensile Strength, Yield 14.5 MPa2100 psiASTM D638
Elongation at Break 1100 %1100 %ASTM D 638
Tensile Modulus 0.127 GPa18.4 ksi1% secant; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 93.0 °C199 °FDSC; LYB Method
Vicat Softening Point 69.0 °C156 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Descriptive Properties
Processing MethodBlown Film, Cast Film, Sheet and Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 1081G Medical Grade EVA
Tisan TISETILEN® Flame Retardant (V0) Polyethylene
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
Braskem TN2020 EVA General Film Copolymer
Baystar™ L425 HDPE Film

PEQT8585 / 220220

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.