MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Celanese Ateva® 1081G Medical Grade EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes:

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³
Vinyl Acetate Content 9.0 %9.0 %
Melt Flow 1.1 g/10 min1.1 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595
Hardness, Shore D 4343
Tensile Strength at Break 17.0 MPa2470 psi
Elongation at Break 700 %700 %
1% Secant Modulus 123 MPa17800 psi
 
Thermal PropertiesMetricEnglishComments
Melting Point 102 °C216 °F
Vicat Softening Point 82.0 °C180 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Antioxidantno
Drug Master Fileyes
Ethylene Oxideyes
Gamma Radiationyes
Steamno

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 1807EG Medical Grade EVA
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
ELASTO UK Mediprene™ 500900M TPE, Medical Applications, 90A Hardness
Celanese Ateva® 2820AG Medical Grade EVA
Celanese 7110 LDPE polymer for medical

PATEVA940 / 170252

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.