MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

European Willow Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Cricket bats, boxes, crates

Key Words: Salix; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.450 g/cc0.0163 lb/in³at 15% Moisture Content
 0.520 g/cc0.0188 lb/in³Air Dry (12-15% Moisture Content)
Cell Length 1.00 mm0.0394 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1600 N360 lb (f)Side
Tensile Strength, Ultimate 2.40 MPa348 psiPerpendicular to Grain
 83.0 MPa12000 psiAxial
Modulus of Rupture 0.0530 GPa7.69 ksiStatic Bending
Flexural Modulus 9.80 GPa1420 ksiStatic Bending
Compressive Strength 3.40 MPa493 psiPerpendicular to Grain
 26.0 MPa3770 psiParallel to Grain
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 6.70 MPa972 psiOrientation Unknown
Toughness 27.6 J20.4 ft-lb2 cm x 2 cm sample
Cleavage 6.40 kN/m36.5 lb/in
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.50 %0.50 %Axial; Green to Zero Moisture
 3.9 %3.9 %Radial; Green to Zero Moisture
 6.8 %6.8 %Tangential; Green to Zero Moisture
 11.5 %11.5 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorPinkish-whiteUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
European Walnut Wood
European Red Oak Wood
European Cherry Wood
European Chestnut Wood
European Hornbeam Wood

PTSE140 / 71323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.