Diffuse-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified. Usual surface texture: Fine Dimensional changes when dried lumber is subjected to variations in humidity during service: Small Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years) Resistance to penetration by preservatives: Resistant Common Applications: Cricket bats, boxes, crates |