MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Glyptal 1212 Aluminum Enamel
Categories: Polymer; Thermoset; Alkyd

Material Notes: GLYPTAL 1212 ALUMINUM ENAMEL is an air-drying or baking general purpose interior and exterior finishing paint. It is GLYPTAL 1202 Varnish furnished with an aluminum paste in a two-compartment container for on-the-job mixing. It has a glossy, brilliant, and metal-like finish with good leafing retention and weather durability.

Suggested Uses: 1212 is suggested for finishing equipment which must stand prolonged temperatures up to 400 ºF. It is ideally suited for the painting of steam lines, ovens, structural iron, wire fencing and exterior piping. It is also suitable for the covering of windows and storage tanks to reflect the sun’s rays.

Application: 1212 may be applied by brush or spray application methods. Proper mixing is obtained by making a smooth paste of the aluminum and approximately 15% of the vehicle and then blending in the rest of the vehicle. Surfaces to be painted should be clean and dry.

Number of Coats: One coat will cover in most applications, but for good exterior weathering, two coats are recommended.

Reduction: Brush: Use at can consistency. Small amounts of mineral spirits may be added if thinning is required. Spray: Should be thinned to 25 sec #2 Zahn Cup with G1500 Thinner.

Surface Preparation: Surfaces to be painted should be dry and free from dirt, wax, grease, rust, and oil. Remove grease and oil by washing surface with mineral spirits. Bare metal surfaces should be primed with 1272 Red Primer.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 52 %52 %Weight
 
Thermal PropertiesMetricEnglishComments
Flash Point 27.2 °C81.0 °F
 
Processing PropertiesMetricEnglishComments
Dry Time 12.0 hour12.0 hourHard
Tack-Free Time 240 min4.00 hourAir Dry
 
Descriptive Properties
ColorAluminum
Coverage450 ft²/galbrush
GlossHigh
RecoatOvernight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silres® SY 300 Silicone Intermediate
Overview of materials for Thermoset Polyurethane, Liquid
Overview of materials for Thermoset Polyurethane, Adhesive
Overview of materials for Silicone Polyurethane, Ether Based
Glyptal 8001 Insulating Enamel

PGLYPT907 / 209746

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.