MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

416 Plus X Martensitic Stainless Steel (UNS S41610)
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Fe-13Cr-2Mn-1Si-0.6Mo-0.15C

Typically used for molds, bearings, turbine components, aircraft structural parts, medical instruments, and cutlery

Key Words: UNS S41610
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 585 - 1210 MPa84800 - 175000 psi
Modulus of Elasticity 204 - 215 GPa29600 - 31200 ksi
Bulk Modulus 166 GPa24100 ksi
Poissons Ratio 0.2830.283
Shear Modulus 83.9 GPa12200 ksi
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.15 %0.15 %
Chromium, Cr 13 %13 %
Iron, Fe 83.25 %83.25 %As Balance
Manganese, Mn 2.0 %2.0 %
Molybdenum, Mo 0.60 %0.60 %
Silicon, Si 1.0 %1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
416 Stainless Steel
416 Stainless Steel, tempered bar
416 Stainless Steel, annealed bar
416 Stainless Steel, tempered and cold drawn bar 25 mm diameter
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600)

MQ416X / 100241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.