MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Ovako S275JR SB1412 Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: S275JR belongs to the group of none alloyed structural steels

Information provided by Ovako

Key Words: St 44-2, SS1414, SS 141412-00
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  410 - 560 MPa
@Thickness <=16.0 mm
59500 - 81200 psi
@Thickness <=0.630 in
Flat bar
 410 - 560 MPa
@Thickness 17.0 - 40.0 mm
59500 - 81200 psi
@Thickness 0.669 - 1.57 in
Flat bar
 410 - 560 MPa
@Thickness 41.0 - 63.0 mm
59500 - 81200 psi
@Thickness 1.61 - 2.48 in
Flat bar
 410 - 560 MPa
@Thickness 64.0 - 80.0 mm
59500 - 81200 psi
@Thickness 2.52 - 3.15 in
Flat bar
Tensile Strength, Yield  >= 245 MPa
@Thickness 64.0 - 80.0 mm
>= 35500 psi
@Thickness 2.52 - 3.15 in
Reh, Flat bar
 >= 255 MPa
@Thickness 41.0 - 63.0 mm
>= 37000 psi
@Thickness 1.61 - 2.48 in
Reh, Flat bar
 >= 265 MPa
@Thickness 17.0 - 40.0 mm
>= 38400 psi
@Thickness 0.669 - 1.57 in
Reh, Flat bar
 >= 275 MPa
@Thickness <=16.0 mm
>= 39900 psi
@Thickness <=0.630 in
Reh, Flat bar
Elongation at Break  20 %
@Thickness 64.0 - 80.0 mm
20 %
@Thickness 2.52 - 3.15 in
Flat bar
 21 %
@Thickness 41.0 - 63.0 mm
21 %
@Thickness 1.61 - 2.48 in
Flat bar
 22 %
@Thickness <=16.0 mm
22 %
@Thickness <=0.630 in
Flat bar
 22 %
@Thickness 17.0 - 40.0 mm
22 %
@Thickness 0.669 - 1.57 in
Flat bar
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 485 °C905 °FMS
 725 °C1340 °FAC1
 863 °C1590 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.21 %<= 0.21 %
Copper, Cu <= 0.55 %<= 0.55 %
Iron, Fe >= 97.25 %>= 97.25 %As Balance
Manganese, Mn <= 1.5 %<= 1.5 %
Nitrogen, N <= 0.012 %<= 0.012 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EN S275JR High Manganese, Structural, Hot Rolled, Base Steel
ASTM A516 Carbon Steel, Grade 70
AISI 1017 Steel, cold drawn
Ovako S235JR EN10025-2 (ref) Steel, +AR
304 Stainless Steel

NOVAKO411 / 234710

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.