Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ERG Aerospace Duocel® Silicon Carbide Foam
Categories: Ceramic; Carbide

Material Notes: Silicon Carbide (SiC) foam is a porous, open-celled structure made from an interconnected lattice of ceramic ligaments. The pattern of cells and ligaments repeats regularly throughout the entirety of the foam, providing uniform material characteristics throughout. The standard Duocel ceramic material is solid, fine grained, Beta phase cubic close packed Silicon Carbide. Other ceramic materials such as Silicon Nitride or Boron Carbide are available on special order.

The resulting foam structure has a high void volume, large surface area, and low flow resistance. It is also lightweight, strong, fracture and thermal shock resistant, and both electrically and thermally conductive. This contrasts strongly with other ceramic foams which are usually relatively fragile and non-conductive. ERG has been supplying Duocel SiC foam for aerospace, defense, and industrial applications since 1980 and has experience with a wide variety of foam applications. Duocel Silicon Carbide can operate effectively up to 2200°C, which makes it suitable for a number of high temperature applications including but not limited to heat exchangers, filters, composite panels, and heat shielding. SiC can endure the extreme conditions that one would expect from solid ceramic materials but at a fraction of the weight.

SiC foam can be used for its fluid flow properties in the etching and deposition stage of semiconductor manufacturing.

Much like RVC foam, Silicon Carbide can be used in electrochemical processes that require low electrical and fluid flow resistance. SiC supplements its strength in this type of application with its increased ability to withstand extreme conditions.

SiC foam can be used in rockets in a multitude of ways, including in the nozzle component where it will be subjected to the exhaust gases that emerge from the motor. As with many other applications, the foam serves two functions, both filtering particulate matter from the exhaust and cooling it as it leaves the rocket.

Silicon Carbide can be used in composite panels and heat shielding elements in many of the same applications that one could expect solid ceramic material to be used.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.161 - 0.385 g/cc0.00582 - 0.0139 lb/in³Typical production range 5 - 12% relative density
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 2.76 - 6.89 GPa400 - 999 ksi
Compressive Yield Strength 1.38 - 5.52 MPa200 - 801 psiVaries directly with relative density (8-16%)
Poissons Ratio 0.220.22
Shear Modulus 1.13 GPa164 ksi
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.200 J/g-°C
@Temperature -150 °C
0.0478 BTU/lb-°F
@Temperature -238 °F
Varies directly with temperature
 1.40 J/g-°C
@Temperature 1450 °C
0.335 BTU/lb-°F
@Temperature 2640 °F
Varies directly with temperature
Thermal Conductivity 1.34 - 2.87 W/m-K
@Temperature 1450 °C
9.30 - 19.9 BTU-in/hr-ft²-°F
@Temperature 2640 °F
Varies directly with relative density (8-16%)
Melting Point 2700 °C4890 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium, Ti
Sandvik 13RM19 Strip Steel
Silicon Carbide, Alpha SiC
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide
CuMoCu 13/74/13

CAERERG02 / 79148

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.