MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Glass Filled

Material Notes: Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature Impact

Uses: Injection Molding

Availability: Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccISO 1183
Filler Content 10 %10 %Glass
 10 %10 %Mineral
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.00060 cm/cm0.00060 in/inflex bar; ASTM D955
 0.0030 cm/cm0.0030 in/inaverage flow and against flow, disc; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 71 - 77
@Time 5.00 sec
71 - 77
@Time 0.00139 hour
ASTM D2240
Tensile Strength 32.0 MPa4640 psiASTM D638
Elongation at Break 39 %39 %ASTM D638
Tensile Modulus 1.90 GPa276 ksiASTM D638
Flexural Strength 41.0 MPa5950 psiASTM D790
Flexural Modulus 1.38 GPa200 ksiASTM D790
Izod Impact, Notched 2.14 J/cm4.00 ft-lb/inASTM D256
 0.374 J/cm
@Temperature -40.0 °C
0.700 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C325 °FASTM D955
Deflection Temperature at 1.8 MPa (264 psi) 122 °C252 °FASTM D955
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 199 °C390 °F
Middle Barrel Temperature 210 °C410 °F
Front Barrel Temperature 221 °C430 °F
Nozzle Temperature 227 °C441 °F
Melt Temperature 227 °C441 °F
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
Injection Pressure 69.0 - 103 MPa10000 - 14900 psi
Hold Pressure 35.0 - 69.0 MPa5080 - 10000 psi
Back Pressure 0.345 MPa50.0 psi
Screw Speed 30 - 80 rpm30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® R 2005/1 20% Glass Filled TPUR
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
Celanese Zenite® 6330 NC010 LCP (Extended Tabular Temperature Data)
Celanese Vectra® A410 Liquid Crystal Polymer (LCP), 25% Glass/25% Mineral Filled

PNOVEON076 / 55341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.