MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro Makrolon® 2407 MAS056 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified; Polycarbonate, Molded; Polycarbonate, UV Stabilized

Material Notes: MVR (300 °C/1.2 kg) 19 cm³/10 min; improved impact strength; low viscosity; UV stabilized; easy release; injection molding - melt temperature 280 - 320 °C; available in light colors only

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 g/cc0.0231 lb/in³pellets; ISO 60
Density 1.20 g/cc0.0434 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.12 %0.12 %ISO 62, 50% RH
Water Absorption at Saturation 0.30 %0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0065 cm/cm
@Thickness 2.00 mm
0.0065 in/in
@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 2.00 mm
0.0070 in/in
@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
20 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  4900 N
@Temperature 23.0 °C
1100 lb (f)
@Temperature 73.4 °F
ISO 6603-2
 5800 N
@Temperature -30.0 °C
1300 lb (f)
@Temperature -22.0 °F
ISO 6603-2
Ball Indentation Hardness 113 MPa16400 psiISO 2039-1
Tensile Strength at Break 65.0 MPa9430 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-1,-2
 115 %115 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 5.8 %5.8 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 93.0 MPa13500 psi2 mm/min; ISO 178
Flexural Yield Strength 72.0 MPa
@Strain 3.5 %
10400 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178
Flexural Strain at Yield 6.8 %6.8 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  16.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
7.61 ft-lb/in²
@Thickness 0.118 in,
Temperature -22.0 °F
complete break; b.o. ISO 180-A
 60.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
28.6 ft-lb/in²
@Thickness 0.118 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature -60.0 °C
NB
@Temperature -76.0 °F
ISO 179-1eU
Charpy Impact, Notched  1.50 J/cm²
@Thickness 3.00 mm,
Temperature -30.0 °C
7.14 ft-lb/in²
@Thickness 0.118 in,
Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 179-1eA
 6.00 J/cm²
@Thickness 3.00 mm,
Temperature 23.0 °C
28.6 ft-lb/in²
@Thickness 0.118 in,
Temperature 73.4 °F
partial break; ISO 7391/b.o. ISO 179-1eA
Puncture Energy  50.0 J
@Temperature 23.0 °C
36.9 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 55.0 J
@Temperature -30.0 °C
40.6 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
864 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VCTI M; Solution B; IEC 60112
 250 V250 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°Fcross-flow; ISO 8302
Hot Ball Pressure Test 136 °C277 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 123 °C253 °FISO 75-1,-2
Vicat Softening Point  143 °C
@Load 5.10 kg
289 °F
@Load 11.2 lb
50°C/h; ISO 306
 144 °C
@Load 5.10 kg
291 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
Flash Point 460 °C860 °FASTM D 1929
 540 °C1000 °Fself ignition; ASTM D 1929
Oxygen Index 30 %30 %Method A; ISO 4589-2
Glow Wire Ignition Temperature  825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
 850 °C
@Thickness 4.00 mm
1560 °F
@Thickness 0.157 in
IEC 60695-2-13
Glow Wire Flammability Index  800 °C
@Thickness 1.00 mm
1470 °F
@Thickness 0.0394 in
IEC 60695-2-12
 800 °C
@Thickness 1.50 mm
1470 °F
@Thickness 0.0591 in
IEC 60695-2-12
 850 °C
@Thickness 2.00 mm
1560 °F
@Thickness 0.0787 in
IEC 60695-2-12
 930 °C
@Thickness 3.00 mm
1710 °F
@Thickness 0.118 in
IEC 60695-2-12
 960 °C
@Thickness 4.00 mm
1760 °F
@Thickness 0.157 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
Electrolytic CorrosionA1IEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2407 MAS070 Polycarbonate
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Covestro Makrolon® 2407 MAS145 Polycarbonate
Covestro Makrolon® 2405 MAS048 Polycarbonate
Albis Plastics ALCOM PC 740 GF23 PTFE 5 , 23% Glass Fiber; 5% PTFE

PB09614 / 150746

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.