MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Albis Plastics ALCOM PC 740 GF23 PTFE 5 , 23% Glass Fiber; 5% PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass + PTFE Filled

Material Notes: Amorphous Polycarbonate (PC)

Characteristics: Low Melt Flow

Applications: Automotive, Construction, Electronic, Lighting, Packaging and Optical Markets

Processing: Injection Molding (Melt Temperature: 540-610°F, Mold Temperature: 150-220°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inASTM D955
Melt Flow 3.1 g/10 min
@Load 1.20 kg,
Temperature 300 °C
3.1 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 69.0 MPa10000 psiASTM D638
Tensile Strength, Yield 62.7 MPa9090 psiASTM D638
Elongation at Break 120 %120 %ASTM D638
Flexural Yield Strength 86.2 MPa12500 psiASTM D790
Flexural Modulus 2.28 GPa331 ksiASTM D790
Izod Impact, Notched 8.54 J/cm16.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FASTM D648
Vicat Softening Point 157 °C315 °F(VST/B/120); ASTM D1525
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Albis Internal Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 282 - 321 °C540 - 610 °FInjection
Mold Temperature 66.0 - 104 °C151 - 219 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2407 MAS056 Polycarbonate
Mitsubishi Iupilon® ECF 2030R Polycarbonate
Aluminum 1050A Composition Spec
Covestro Makrolon® 2805 MAS152 Polycarbonate
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite

PZA1B53 / 21740

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.