MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco Polystar® RB NLGI Grade 2
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Texaco Polystar RB 2 delivers value through:
  • Ability to meet bearing OEM requirements — Suitable for high rpm operations, operating temperatures ranging from -34°C to 204°C (-30°F to 400°F) and offers excellent rust protection in the presence of both salt and fresh water.
  • Excellent oxidation stability — Provides excellent bearing life with continuous service possible at temperatures up to 160°C (320°F). For short exposure, the maximum is 200°C (392°F).
  • Corrosion protection — Provides superior water resistance and protection of bearings against rust and corrosion.
  • Good low shear stability — Will not soften excessively under prolonged low shear stress.

Texaco Polystar RB 2 is a high temperature ball and roller bearing grease.

It is formulated with high quality base stocks, a synthetic polyurea ashless organic thickener, and high performance rust and oxidation inhibitors (the latter to provide superior rust protection in severe applications).

Texaco Polystar RB 2 is specifically designed to meet the factory-fill performance requirements of the major manufacturers of rolling element bearings.

Texaco Polystar RB 2 is recommended:

  • For use in antifriction bearings operating at high speeds (speeds up to 500,000 DN).
  • Where the operating temperatures are on the order of 150°C (302°F) and higher.
  • Where there is a likelihood that water or salt water will get into the bearings.

It performs satisfactorily in bearings at temperatures as low as -34°C (-30°F).

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 221915; MSDS Number: 8998

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9595Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 607 SUS607 SUSSee Note 3.
Saybolt Viscosity at 210°F 68 SUS68 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 116 cSt116 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 12.2 cSt12.2 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Penetration P(60), 1/10 mm 280280Unknown Amount of Work, 25°C (77°F)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FSee Note 2.
Minimum Service Temperature, Air -34.0 °C-29.2 °FSee Note 1.
Flash Point >= 209 °C>= 408 °F
Dropping Point 260 °C500 °F
 
Descriptive Properties
ColorPurple
Rust PreventionPassModified 5% Synthetic sea water
TextureSmooth, Buttery
Thickener, %12Polyurea

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) RHODOLINE® 4200 Surfactant
ChevronTexaco Polystar® Synthetic 4602 NLGI Grade
ChevronTexaco Polystar® CVJ

WTEXA264 / 77143

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.