MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: Chromium-molybdenum-tungsten-vanadium alloyed PM steel

Vanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications where wear resistance above that of an ORVAR 2M / AISI H13 is required. This material is available in limited sizes.

Vanadis 23 is characterized by:

  • High wear resistance (abrasive profile)
  • High compressive strength
  • Very good through-hardening properties
  • Good toughness
  • Very good dimensional stability on heat treatment
  • Very good temper resistance
Applications: Uddeholm Vanadis 23 is especially suitable for blanking and forming of thinner work materials where a mixed (abrasive–adhesive) or abrasive type of wear is encountered and where the risk for plastic deformation of the working surfaces of the tool is high, e.g.:Blanking of medium to high carbon steel
  • Blanking of harder materials such as hardened or cold-rolled strip steel
  • Plastics mould tooling subjected to abrasive wear condition
  • Plastics processing parts, e.g. feed screws, barrel liners, nozzles, screw tips, non-return check ring valves, pellitizer blades, granulator knives

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.94 g/cc0.287 lb/in³hardened and tempered
     7.78 g/cc
    @Temperature 599 °C
    0.281 lb/in³
    @Temperature 1110 °F
    hardened and tempered
     7.83 g/cc
    @Temperature 399 °C
    0.283 lb/in³
    @Temperature 750 °F
    hardened and tempered
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Brinell 260260Soft annealed (Delivery condition)
    Hardness, Rockwell C 57 - 6657 - 66Tempering: 3 x 1 h at 1040°F
    Modulus of Elasticity 228 GPa33000 ksi(hardened and tempered)
     186 GPa
    @Temperature 599 °C
    27000 ksi
    @Temperature 1110 °F
    hardened and tempered
     207 GPa
    @Temperature 399 °C
    30000 ksi
    @Temperature 750 °F
    hardened and tempered
    Flexural Strength 5000 MPa725000 psi(Fracture) @58HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
     5300 MPa769000 psi(Fracture) @62HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
    Flexural Yield Strength 2700 MPa392000 psi@58HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
     3500 MPa508000 psi@64HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
    Impact Test 33.9 - 56.9 J25.0 - 42.0 ft-lbunnotched; Tempering: 3 x 1 h at 1040°F
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  12.1 µm/m-°C
    @Temperature 399 °C
    6.70 µin/in-°F
    @Temperature 750 °F
    hardened and tempered
     12.6 µm/m-°C
    @Temperature 599 °C
    7.00 µin/in-°F
    @Temperature 1110 °F
    hardened and tempered
    Specific Heat Capacity 0.418 J/g-°C0.100 BTU/lb-°Fhardened and tempered
     0.502 J/g-°C
    @Temperature 399 °C
    0.120 BTU/lb-°F
    @Temperature 750 °F
    hardened and tempered
     0.586 J/g-°C
    @Temperature 599 °C
    0.140 BTU/lb-°F
    @Temperature 1110 °F
    hardened and tempered
    Thermal Conductivity 24.0 W/m-K167 BTU-in/hr-ft²-°Fhardened and tempered
     27.0 W/m-K
    @Temperature 599 °C
    187 BTU-in/hr-ft²-°F
    @Temperature 1110 °F
    hardened and tempered
     28.0 W/m-K
    @Temperature 399 °C
    194 BTU-in/hr-ft²-°F
    @Temperature 750 °F
    hardened and tempered
    Shrinkage -0.130 - -0.0300 %-0.130 - -0.0300 %Austenitizing and tempering
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 1.28 %1.28 %
    Chromium, Cr 4.2 %4.2 %
    Iron, Fe 80.02 %80.02 %As Balance
    Molybdenum, Mo 5.0 %5.0 %
    Tungsten, W 6.4 %6.4 %
    Vanadium, V 3.1 %3.1 %
     
    Descriptive Properties
    Deflection, mm2.1@64HRC, Tempering: 3 x 1 h at 1040°F
     3.7@58HRC, Tempering: 3 x 1 h at 1040°F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Assab Steels ASP 23 Cold Work Steel
    Crucible Steel CPM® 10V® (AISI A11) Tool Steel
    Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
    AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
    AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)

    NBUCOR08 / 15477

    New MatWeb Services

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.