MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CHT Group QGel 319 Optically Clear Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QGel 319 is an optically clear, moderately cross-linked silicone potting compound. Silicone potting compounds are used to provide protection from vibration and thermal or mechanical shock.

Key Features:

  • 10:1 mix ratio
  • 24 hour room temperature cure
  • Soft, but has considerably higher strength than general purpose silicone gels
  • Dispensing equipment not necessary

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccUncatalyzed A
 0.970 g/cc0.970 g/ccUncatalyzed B
Viscosity 900 cP900 cPUncatalyzed A
 3200 cP3200 cPUncatalyzed B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2020Cured 30 min. at 150°C
Tensile Strength 0.414 MPa60.0 psiCured
Elongation at Break 120 %120 %Cured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1200 min20.0 hour
 30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 60.0 min
@Temperature 100 °C
1.00 hour
@Temperature 212 °F
Gel Time 120 min120 minCatalyzed
 
Descriptive Properties
ColorTransparentUncatalyzed A
 TransparentUncatalyzed B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
CHT Group QGel 311 UV Special Purpose Silicone Gel
CHT Group QGel 314 General Purpose Silicone Gel
CHT Group QGel 315 QSI Quantum Silicones General Purpose Silicone Gel
CHT Group QGel 322 General Purpose Silicone Gel

PACC2019 / 199407

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.