MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QGel 315 QSI Quantum Silicones General Purpose Silicone Gel
Categories: Fluid; Polymer; Thermoset; Silicone

Material Notes: QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection.

Key Features:

  • 24 hour room temperature cure
  • One to one mix ratio
  • Soft but resilient
  • Heat cure required
Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/cc"B" component
 0.970 g/cc0.970 g/cc"A" component
Viscosity 1000 cP1000 cP"B" component
 1000 cP1000 cP"A" component
Storage Temperature <= 38.0 °C<= 100 °F12 months
 
Mechanical PropertiesMetricEnglishComments
Penetration 5.0 - 9.05.0 - 9.0mm, 30 mins @ 150°C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 - 30.0 min
@Temperature 150 °C
0.250 - 0.500 hour
@Temperature 302 °F
 45.0 - 60.0 min
@Temperature 100 °C
0.750 - 1.00 hour
@Temperature 212 °F
 120 - 240 min
@Temperature 25.0 °C
2.00 - 4.00 hour
@Temperature 77.0 °F
Gel Time >= 1440 min>= 1440 min
 
Descriptive Properties
ColorTransparent"A" component
 Transparent"B" component

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QGel 319 Optically Clear Silicone Gel
CHT Group QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
CHT Group QSil 551 QSI Quantum Silicones Silicone Potting Material
CHT Group QGel 312 Custom Silicone Gel
CHT Group QGel 311 UV Special Purpose Silicone Gel

PACC046 / 22173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.