MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, dry  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Cable Sheathing Grade

Material Notes: Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact resistance, high burst pressure, low gasoline permeation, and good chemical resistance. It is widely used for auto fuel lines, air brake tubing, cable sheathing et al and meets ISO 7628, DIN 73378, DIN 74324 standards in automotive industry.

Information provided by Suzhou Hipro Polymers Co. Ltd., subsequently acquired by Arkema S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Water Absorption 1.6 %1.6 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiISO 527-1/-2
Tensile Modulus 0.330 GPa47.9 ksiISO 527-1/-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 182 °C360 °FISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO75-1/-2
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 250 °C374 - 482 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 4 hour4 hour
Moisture Content <= 0.10 %<= 0.10 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, conditioned
Suzhou Hipro Polymers Hiprolon® 11 PES Colorized Nylon powder
Evonik VESTAMID® NRG 2101 PA 12
Ashley Polymers Ashlene® T940H Nylon 11
Arkema Rilsan® MB 3610 NAT PA11-I

PHIPRO03 / 106818

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.