MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Suzhou Hipro Polymers Hiprolon® 11 PES Colorized Nylon powder  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11)

Material Notes: Hiprolon® 11 PES colorized electrostatic polyamide powder is partly comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistance, and superior adhesion strength with metal surfaces. It is widely used for coating of auto parts, hard wares, water pipes racks et al. Available in various colors to provide a customized product. It can be applied to subjects with a 0.7mm-0.3mm thickness range, and it can also achieve a thinner thickness when it is not coated by dipping. The optimal coating thickness is 0.12-0.15mm.

Information provided by Suzhou Hipro Polymers Co. Ltd., subsequently acquired by Arkema S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Water Absorption 0.90 %0.90 %ISO 62
Particle Size <= 80 µm<= 80 µm> 99 wt.%; DIN EN ISO 4610
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ISO 868
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmISO 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmISO 60093
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 160 °C320 °FISO 306
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
ISO1210
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
ISO1210
 
Descriptive Properties
Salt Spray Resistance< 1mm corrosionISO 7253; Testing according to WIS 4-52-01; 2000 hours

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, conditioned
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, dry
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, conditioned
Arkema Rilsan® MB 3610 NAT PA11-I
Arkema Rilsan® BMNO TEX PA11

PHIPRO05 / 106820

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.