MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Zelux® CN-P Polycarbonate (conductive)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Conductive

Material Notes: Zelux® CN-P is a conductive, carbon powder filled polycarbonate (PC). This product offers surface resistivity of 10E5 - 10E7 ohm/sq. Zelux® CN-P has low outgassing properties, high flexural strength, and good thermal stability to 250°F. Zelux® CN-P offers UL94 V-0 performance down to 0.030" and is thermoformable.

Colors Available: Black

Attributes: Dielectric Properties; Dimensional Stability

Shapes: Compression Sheet; Extruded Rod; Extruded Film

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Water Absorption 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM D2240
Tensile Strength, Yield 65.0 MPa9430 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Strength 107 MPa15500 psiASTM D790
Flexural Modulus 3.172 GPa460.1 ksiASTM D790
Izod Impact, Notched 0.747 J/cm1.40 ft-lb/inASTM D256
Izod Impact, Unnotched 5.34 J/cm10.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 - 1.00e+6 ohm-cm1000 - 1.00e+6 ohm-cm< 0.1 seconds; ASTM D257
Surface Resistance 1000 - 1.00e+6 ohm1000 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.762 mm
V-0
@Thickness 0.0300 in
 
Descriptive Properties
ColorBlack
Compression Sheet Sizing48" Length by 24" Width0.25", 0.5", 0.75", 1", 1.25", 1.5", 1.75", 2", 2.25", 2.5", 2.75", 3", 3.25", 3.5", 3.75", 4"
Extruded Sheet Sizing96" Length by 48" Width0.03", 0.035", 0.06", 0.08", 0.09", 0.09", 0.095", 0.125", 0.1875", 0.25"
Film Sizing26" Width0.005", 0.01" 0.02"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable 3311-xx23D Polyvinyl Chloride, Flexible
Ensinger Tecanat™ Unfilled Polycarbonate (PC)
Ensinger Tecanat™ GF20 20% Glass Reinforced Polycarbonate (PC)
Mitsubishi Chemical Advanced Materials Altron™ PC Extruded, Unfilled, Polycarbonate
Overview of materials for Polycarbonate, UV Stabilized

PWEST055 / 72735

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.