System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Thermx® TE3002 BK010 PCT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polycyclohexylenedimethylene Terephthalate (PCT)
;
Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
Material Notes:
Thermx® TE3002 BK010 is a 30% glass fiber reinforced, flame retardant, black high performance polyester resin for injection molding.
Celenese acquired the Thermx product line from DuPont in 2010.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.65
g/cc
0.0596
lb/in³
ISO 1183
Filler Content
30 %
30 %
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
100
MPa
14500
psi
ISO 527
Elongation at Break
1.2 %
1.2 %
ISO 527
Tensile Modulus
10.0
GPa
@Temperature 23.0 °C
1450
ksi
@Temperature 73.4 °F
ISO 527
Flexural Strength
150
MPa
21800
psi
ISO 178
Flexural Modulus
10.5
GPa
1520
ksi
ISO 178
Charpy Impact Unnotched
2.00
J/cm²
@Temperature 23.0 °C
9.52
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.700
J/cm²
@Temperature 23.0 °C
3.33
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
240
°C
464
°F
ISO 75-1/-2
UL RTI, Electrical
150
°C
@Thickness 1.50 mm
302
°F
@Thickness 0.0591 in
UL 746B
150
°C
@Thickness 0.790 mm
302
°F
@Thickness 0.0311 in
UL 746B
150
°C
@Thickness 3.00 mm
302
°F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical without Impact
140
°C
@Thickness 0.790 mm
284
°F
@Thickness 0.0311 in
UL 746B
150
°C
@Thickness 3.00 mm
302
°F
@Thickness 0.118 in
UL 746B
150
°C
@Thickness 1.50 mm
302
°F
@Thickness 0.0591 in
UL 746B
Flammability, UL94
V-0
@Thickness 0.790 mm
V-0
@Thickness 0.0311 in
IEC 60695-11-10
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
V-0
@Thickness 0.790 mm
V-0
@Thickness 0.0311 in
UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL94
V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10
V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL94
Processing Properties
Metric
English
Comments
Melt Temperature
300
°C
572
°F
Optimum
295
-
310
°C
563
-
590
°F
Mold Temperature
100
°C
212
°F
Optimum
80.0
-
120
°C
176
-
248
°F
Drying Temperature
95.0
°C
203
°F
Dry Time
4
-
6
hour
4
-
6
hour
Dehumidified Dryer
Moisture Content
<= 0.030 %
<= 0.030 %
Descriptive Properties
Color
Black
Drying Recommended
Yes
Filler
Glass Reinforced
Forms
Pellets
Generic
PCT
Part Marking Code
>PCT-GF30FR(17)<
ISO 11469
Polymer Family
Polyester
Polymer Type
PCT
Processing Method
Injection Molding
Product Category
Flame Retardant Resins
Glass Reinforced Resins
Region Available
Americas
Asia/Pacific
Europe
Resin Identification
PCT-GF30FR(17)
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Thermx® CG023 NC010 PCT
Celanese Thermx® TE1001 BK010 PCT
Celanese Thermx® CG923 BK010 PCT
Celanese Thermx® LED 0201 PCT, 40% Specialty
Celanese Thermx® LED 0201S PCT, 38% Specialty
PDTA7740 / 89901
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.