MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AK Steel 400 Ferritic Stainless steel
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: AK Steel 400 is one of the most economical chromium ferritic stainless steels. It has corrosion and oxidation resistance comparable to Type 410 stainless steel with good fabricating characteristics. AK Steel 400 contains no titanium, so its surface is free of titanium streaks. This provides improved appearance, and alleviates die wear that may be caused by titanium stabilized chromium steels. AK Steel 400 is non-hardenable by heat treatment because of its low carbon content which also minimizes hardening during welding. Typical applications include heat exchangers, display racks, gas range burner rings, office furniture and other uses where corrosion resistance at minimum cost is important.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.47 g/cc0.270 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7272
Tensile Strength, Ultimate 469 MPa68000 psi
Tensile Strength, Yield 234 MPa
@Strain 0.2 %
33900 psi
@Strain 0.2 %
Elongation at Break 30 %30 %in 2 inches
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000600 ohm-cm0.0000600 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.8 µm/m-°C
@Temperature 24.0 - 260 °C
6.00 µin/in-°F
@Temperature 75.2 - 500 °F
 12.8 µm/m-°C
@Temperature <=871 °C
7.11 µin/in-°F
@Temperature <=1600 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  24.9 W/m-K
@Temperature 100 °C
173 BTU-in/hr-ft²-°F
@Temperature 212 °F
 28.6 W/m-K
@Temperature 500 °C
198 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.25 %<= 0.25 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 12 - 13 %12 - 13 %
Iron, Fe >= 84.64 %>= 84.64 %As Remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 440 Stainless Steel
Overview of materials for T 400 Series Stainless Steel
AK Steel 430 Ferritic Stainless steel
AK Steel 420 Martensitic Stainless steel
AK Steel 409 Ferritic Stainless steel

NAKS092 / 14695

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.