MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Quentys™ SF700CL Polyolefin, Talcum Filled
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Quentys™ SF700CL is a polyolefin based talcum filled compound. SF700CL in combination with other PP based compounds improves the recyclability of PV modules.

Special Features: Quentys SF700CL has a good dimensional and thermal stability, and displays a high resistance to hydrolysis under hot and humid conditions. Quentys SF700CL is furthermore resistant to UV without protective fluorinated layers and demonstrates good adhesion to Ethyl Vinyl Acetate (EVA) encapsulant film.

Applications: Quentys SF700CL is suitable for (thick) film extrusion for core layer in solar backsheet application.

Specifications: Quentys SF700CL when used as core layer is expected to meet the backsheet requirements included in the below mentioned standards provided it is processed using sound material handling, extrusion practices as well as appropriate testing procedures. EN ISO 4892-2; IEC 60215-2: 2016; IEC 60216-5; IEC 60243-1; IEC 60664-1: 2007 clause 6, 1, 3, 5; IEC 61730-2: 2016; IEC 62701 clause 7, 8, 10; IEC 62716 clause 7, 8, 10

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183-1/A
Melt Flow 7.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 35.0 °C<= 95.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 17.0 MPa>= 2470 psiISO 527-3
Tensile Modulus >= 1.40 GPa>= 203 ksiISO 527-3
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9882 / 323239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.