MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel CPM® S90V® (420V®) Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Martensitic; Tool Steel

Material Notes: CPM S90V is a unique tool steel made by the Crucible Particle Metallurgy process. It is a martensitic stainless steel with a high volume of vanadium carbides for exceptionally good wear resistance. S90V offers substantial improvements in wear resistance over 440C and D2, and other high chromium tool steels, with corrosion resistance equal to or better than 440C. Its high vanadium content favors the formation of hard vanadium carbides instead of chromium carbides for wear resistance, leaving sufficient chromium in the matrix to provide good corrosion resistance.

The wear and corrosion resistance of S90V make it an excellent candidate to replace 440C, where increased wear is a primary concern. It can replace D2 or other tool steels in applications where improved corrosion resistance is also of benefit.

The CPM process results in a finer, more uniform carbide distribution imparting improved toughness and grindability to high alloy steels. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.40 g/cc0.267 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 277277Annealed
Hardness, Rockwell C 56 - 5956 - 59
Modulus of Elasticity 215 GPa31200 ksi
Charpy Impact 27.12 J20.00 ft-lb
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 200 °C
6.11 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 17.3 W/m-K
@Temperature 65.0 °C
120 BTU-in/hr-ft²-°F
@Temperature 149 °F
Shrinkage -0.0500 - -0.0300 %-0.0500 - -0.0300 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.3 %2.3 %
Chromium, Cr 14 %14 %
Iron, Fe 73.7 %73.7 %As Remainder
Tungsten, W 1.0 %1.0 %
Vanadium, V 9.0 %9.0 %
 
Descriptive Properties
Corrosion Rate; mm/y102 to 117Dilute Aqua-Regia
 9 to 1710% Boiling Acetic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CPM® S35VN™ Stainless Steel
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
Crucible Steel CPM® 9V® Tool Steel
Crucible Steel CPM® S110V® Stainless Tool Steel
420 Stainless Steel, hardened and tempered bar

NCRUC013 / 16006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.