MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Phenolic, Novolac, Fabric Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Fabric Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.45 g/cc0.0415 - 0.0524 lb/in³Average value: 1.36 g/cc Grade Count:31
Water Absorption 0.300 - 1.10 %0.300 - 1.10 %Average value: 0.706 % Grade Count:12
Linear Mold Shrinkage 0.00150 - 0.00400 cm/cm0.00150 - 0.00400 in/inAverage value: 0.00267 cm/cm Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 76.0 - 86.076.0 - 86.0Average value: 79.3 Grade Count:3
Hardness, Rockwell M 98.0 - 11298.0 - 112Average value: 107 Grade Count:4
Ball Indentation Hardness 130 - 170 MPa18900 - 24700 psiAverage value: 147 MPa Grade Count:7
Tensile Strength, Ultimate 41.0 - 58.0 MPa5950 - 8410 psiAverage value: 50.5 MPa Grade Count:11
Tensile Strength, Yield 40.0 - 100 MPa5800 - 14500 psiAverage value: 63.3 MPa Grade Count:9
Modulus of Elasticity 6.00 - 8.00 GPa870 - 1160 ksiAverage value: 7.14 GPa Grade Count:7
Flexural Yield Strength 60.0 - 180 MPa8700 - 26100 psiAverage value: 93.1 MPa Grade Count:27
Flexural Modulus 7.00 - 11.0 GPa1020 - 1600 ksiAverage value: 9.34 GPa Grade Count:10
Compressive Yield Strength 80.0 - 320 MPa11600 - 46400 psiAverage value: 144 MPa Grade Count:31
Izod Impact, Notched 0.683 - 1.44 J/cm1.28 - 2.71 ft-lb/inAverage value: 1.02 J/cm Grade Count:11
Izod Impact, Notched (ISO) 8.00 - 55.0 kJ/m²3.81 - 26.2 ft-lb/in²Average value: 19.9 kJ/m² Grade Count:9
Coefficient of Friction 0.0200 - 0.2000.0200 - 0.200Average value: 0.0650 Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+8 ohm1.00e+8 ohmAverage value: 1.00e+8 ohm Grade Count:5
Insulation Resistance 100000 - 2.00e+7 ohm100000 - 2.00e+7 ohmAverage value: 4.44e+6 ohm Grade Count:10
Dielectric Constant 5.00 - 10.05.00 - 10.0Average value: 6.00 Grade Count:6
Dielectric Strength 8.70 - 20.0 kV/mm221 - 508 kV/inAverage value: 12.4 kV/mm Grade Count:10
Dielectric Breakdown  >= 1000 V
@Temperature 90.0 - 90.0 °C
>= 1000 V
@Temperature 194 - 194 °F
Average value: 7220 V Grade Count:9
 >= 1000 V
@Time 20.0 - 60.0 sec
>= 1000 V
@Time 0.00556 - 0.0167 hour
Average value: 7220 V Grade Count:9
Dielectric Loss Index 0.300 - 0.4000.300 - 0.400Average value: 0.340 Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 40.0 µm/m-°C8.33 - 22.2 µin/in-°FAverage value: 29.2 µm/m-°C Grade Count:11
Thermal Conductivity 0.290 - 0.300 W/m-K2.01 - 2.08 BTU-in/hr-ft²-°FAverage value: 0.296 W/m-K Grade Count:7
Maximum Service Temperature, Air 120 - 150 °C248 - 302 °FAverage value: 136 °C Grade Count:11
Deflection Temperature at 1.8 MPa (264 psi) 121 - 260 °C250 - 500 °FAverage value: 196 °C Grade Count:10
 
Processing PropertiesMetricEnglishComments
Mold Temperature 150 - 180 °C302 - 356 °FAverage value: 164 °C Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
Overview of materials for Phenolic/Glass Fiber SMC
Overview of materials for Polycarbonate, Extruded
Hippe PF CC 21 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube
Overview of materials for Phenolic, Novolac, Cellulose Filled

O2738 / 78101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.