MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aluminum 1060-H112
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Key Words: UNS A91060; AA1060-H112; Al1060-H112
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.705 g/cc0.09772 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 58.0 - 95.0 MPa8410 - 13800 psiExtruded tube
 >= 58.0 MPa
@Thickness 0.254 - 12.7 mm
>= 8410 psi
@Thickness 0.0100 - 0.500 in
Drawn tube
 >= 62.0 MPa
@Thickness 25.43 - 76.2 mm
>= 8990 psi
@Thickness 1.001 - 3.00 in
Sheet and plate
 >= 70.0 MPa
@Thickness 12.7 - 25.4 mm
>= 10200 psi
@Thickness 0.500 - 1.00 in
Sheet and plate
 >= 75.0 MPa
@Thickness 6.35 - 12.7 mm
>= 10900 psi
@Thickness 0.250 - 0.499 in
Sheet and plate
Tensile Strength, Yield >= 17.0 MPa>= 2470 psiExtruded tube
 >= 17.0 MPa
@Thickness 0.254 - 12.7 mm
>= 2470 psi
@Thickness 0.0100 - 0.500 in
Drawn tube
Elongation at Break  >= 10 %
@Thickness 6.35 - 12.7 mm
>= 10 %
@Thickness 0.250 - 0.499 in
Sheet and plate
 >= 20 %
@Thickness 12.7 - 25.4 mm
>= 20 %
@Thickness 0.500 - 1.00 in
Sheet and plate
 >= 25 %
@Thickness 25.43 - 76.2 mm
>= 25 %
@Thickness 1.001 - 3.00 in
Sheet and plate
 >= 30 %
@Thickness 1.27 - 4.29 mm
>= 30 %
@Thickness 0.0500 - 0.169 in
Extruded tube
Modulus of Elasticity 69.0 GPa10000 ksi
Poissons Ratio <= 0.33<= 0.33
Shear Modulus 25.9 GPa3760 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 234 W/m-K1620 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 99.6 %>= 99.6 %Specified
Copper, Cu <= 0.050 %<= 0.050 %
Iron, Fe <= 0.35 %<= 0.35 %
Magnesium, Mg <= 0.030 %<= 0.030 %
Manganese, Mn <= 0.030 %<= 0.030 %
Other, each <= 0.030 %<= 0.030 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.030 %<= 0.030 %
Vanadium, V <= 0.050 %<= 0.050 %
Zinc, Zn <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 1060-O
Aluminum 1060-H18
Aluminum 1060-H12
Aluminum 1060-H16
Aluminum 1060-H14

MA1060H112 / 109157

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.