MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum 1060-H112
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Key Words: UNS A91060; AA1060-H112; Al1060-H112
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.705 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 58.0 - 95.0 MPaExtruded tube
 >= 58.0 MPa
@Thickness 0.254 - 12.7 mm
Drawn tube
 >= 62.0 MPa
@Thickness 25.43 - 76.2 mm
Sheet and plate
 >= 70.0 MPa
@Thickness 12.7 - 25.4 mm
Sheet and plate
 >= 75.0 MPa
@Thickness 6.35 - 12.7 mm
Sheet and plate
Tensile Strength, Yield >= 17.0 MPaExtruded tube
 >= 17.0 MPa
@Thickness 0.254 - 12.7 mm
Drawn tube
Elongation at Break >= 10 %
@Thickness 6.35 - 12.7 mm
Sheet and plate
 >= 20 %
@Thickness 12.7 - 25.4 mm
Sheet and plate
 >= 25 %
@Thickness 25.43 - 76.2 mm
Sheet and plate
 >= 30 %
@Thickness 1.27 - 4.29 mm
Extruded tube
Modulus of Elasticity 69.0 GPa
Poissons Ratio <= 0.33
Shear Modulus 25.9 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.900 J/g-°C
Thermal Conductivity 234 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al >= 99.6 %Specified
Copper, Cu <= 0.050 %
Iron, Fe <= 0.35 %
Magnesium, Mg <= 0.030 %
Manganese, Mn <= 0.030 %
Other, each <= 0.030 %
Silicon, Si <= 0.25 %
Titanium, Ti <= 0.030 %
Vanadium, V <= 0.050 %
Zinc, Zn <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 1060-O
Aluminum 1060-H18
Aluminum 1060-H12
Aluminum 1060-H16
Aluminum 1060-H14

MA1060H112 / 109157

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.