MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives

Unit of Measure Converter

Unit Converter
Equivalent Values
UOM Value
cable lengths 0.00143
chains (Gunter's) 0.0154
cubits 0.678
fathoms 0.170
ft 1.02
furlongs 0.00155
hands 3.05
in 12.2
km 0.000310
leagues 0.0000620
leagues (nautical) 0.0000620
links (Gunter's) 1.54
links (Ramden's) 1.02
m 0.310
microns 310000
mil 12200
miles (nautical, Int.) 0.000167
miles (statute) 0.000193
mm 310
nm 3.10e+8
picas 73.5
points 882
rods 0.0616
spans 1.36
varas 0.366
yards 0.339
 

MatWeb has also provided a reference table for converting between English and Metric units.

To Convert From: To: Multiply By:
lbf/in2 (psi) pascal (Pa) 6894.757
pascal (Pa) lbf/in2 (psi) 1.4504E-4
g/cm3 lb/ft3 62.427974
lb/ft3 kg/m3 16.01846
lb/in3 kg/m3 27,679.90
lb/ft3 g/cm3 0.01601846
volts/mil kV/mm 0.039370
mil (0.001 inch) cm 2.54E-3
cm mil 393.70
MPa(m1/2) psi(in1/2) 910.06
J/(g-°C) BTU/(lb-°F) 0.239006
BTU/(lb-°F) J/(g-°C) 4.184000
joule (J) cal (thermochemical) 0.2390057
cal (thermochemical) joule (J) 4.184000
joule (J) BTU (thermochemical) 9.4845E-4
BTU (thermochemical) joule 1054.350
µm/(m-°C) µin/(in-°F) 0.55556
µin/(in-°F) µm/(m-°C) 1.80
cm3/Kg in3/lb 0.027680
in3/lb cm3/kg 36.127
W/(m K) BTU in /(hr ft2  F) 6.9334713
BTU in /(hr ft2  F) W/(m K) 0.1441314
(J m)/(min m2  C) W/(m-K) 0.016667
W/(m-K) (J m)/(min m2  C) 60
© MatWeb:  This table may be copied, but the copyright and hyperlink to MatWeb must not be removed.
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.