MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Innegra™ Techologies Innegra™ S IS-2800 Olefinic Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer

Material Notes: Innegra S is an olefin based high performance yarn used most often in conjunction with a high modulus fiber to increase toughness, durability, dampening, and in some cases, reduce weight.

When high modulus fibers are combined with Innegra™ S fiber, weight can be reduced, impact resistance, damage tolerance and signal transmission vastly improved, expanding the performance of existing materials. Properties of Innegra™S Fiber include:

  • Multi-filament, high modulus olefin yarn
  • Hydrophobic
  • Tough
  • Ductile
  • Durable
  • Low Dielectric Properties
  • Low Elongation
  • Low Creep
  • Highly Crystalline
  • Recyclable
Available in white or black

Information provided by Innegra Technologies.

Vendors:
Available Properties
  • Density
  • Fiber Count, ASTM D1907
  • Tensile Strength, Ultimate, ASTM D885, Using density of 0.84 g/cc
  • Elongation at Break, ASTM D885
  • Tensile Modulus, ASTM D885, Using density of 0.84 g/cc
  • Tenacity, ASTM D885
  • Dielectric Constant
  • Dielectric Loss Index
  • Maximum Service Temperature, Air, DSC; Processing/Service Limit
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.