MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
PolyMirae Clyrell EC310K Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Clyrell EC310K is a medium flow heterophasic copolymer selected by customers for use in film applications. Films produced with Clyrell EC310K shows very good gel level and good heat seal properties. Clyrell EC310K films are also characterized by an excellent balance of toughness, low temperature impact, mechanical properties, easy processing and low stress whitening. Clyrell EC310K is typically used by customers for lamination, adhesive tapes, labeling films, thermoformed containers, stationery and protective films and food packaging. Clyrell EC310K contains no slip or antiblocking agents. Clyrell EC310K is suitable for food contact.

Product Features: Very low gel content/Absence of film stress whitening/ Good film stiffness with low temperature impact/ Low blooming even after ageing/ Good seal strength/ Good optical properties/High heat resistance

Typical Applications: Extrusion of films for lamination/Adhesive tapes/ Labeling films/Thermoformed containers /Stationery /Protective films /Food packaging

Information provided by PolyMirae

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASMT D1238, Condition L
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
PolyMirae Company Ltd.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.