MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
DIAB Divinycell® HP 100 Sandwich Core Material
Categories: Other Engineering Material; Composite Core Material; Polymer

Material Notes: Divinycell HP has been developed to be fully compatible with low and medium temperature prepreg and RFI systems. Divinycell HP's elevated temperature performance also extends to its 'in service' life as it will retain a high percentage of its mechanical properties despite exposure to high ambient temperatures.

The mechanical properties of Divinycell HP have not been compromised in order to achieve its elevated temperature performance. It offers higher values than other commonly used 'elevated temperature cores' in all significant areas including its strength properties, elongation to break, ductility, adhesion/peel strength, fracture toughness and dimensional stability. Other key features of Divinycell HP include excellent chemical resistance (including styrene), low water absorption and good thermal/acoustic insulation.

Continuous operating temperature is -200 to 80°C. The foam can be used in sandwich structures, for outdoor exposure, with external skin temperatures up to 100°C. Normally Divinycell HP can be processed up to 145°C with minor dimensional changes. Maximum processing temperature is dependent on time, pressure and process conditions.

Information Provided by DIAB

Vendors:
Available Properties
  • Density, ISO 845
  • Tensile Strength, Ultimate, ASTM D1623, Perpendicular to the plane
  • Elongation at Break, ASTM C273, In Shear
  • Tensile Modulus, ASTM D1623, Perpendicular to the plane
  • Compressive Strength, ASTM D1621, Perpendicular to the plane
  • Compressive Modulus, ASTM D1621, Perpendicular to the plane
  • Shear Modulus, ASTM C273
  • Shear Strength, ASTM C273
  • CTE, linear
  • Maximum Service Temperature, Air, Continuous
  • Minimum Service Temperature, Air, Continuous
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DIAB Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.