| The high-strength structural steel SSAB Docol S960MC is a hot-rolled steel made for cold forming, with a minimum yield strength of 960 MPa. SSAB Docol S960MC meets or exceeds the requirements of S960MC in EN 10149-2. SSAB Docol S960MC is provided as cut-to-length sheets with excellent thickness accuracy and surface quality. Typical applications include a wide range of components and parts for lighter transport solutions. Dimension Range: SSAB Docol S960MC is available as cut to length sheets with mill edge in thicknesses of 3.00 - 10.00 mm, widths up to 1600 mm and lengths up to 13 meters. Data provided by SSAB. |