MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity is essential. This two-part system remains at a constant viscosity for a minimum of 50 minutes. This allows more connectors to be produced from a single lot. It is a very high strength adhesive that will not distort plastic fibers. TRA-BOND F109CLR can be cured at room temperature overnight or as fast as 20 minutes at 65°C. This 100% solid system can be used for small potting and sealing applications where thermal shock and impact resistance are required. Fully cured TRA-BOND F109CLR provides excellent resistance to salt solutions, mild acids, alkalis and many other chemicals including petroleum solvents and alcohol. TRA-BOND F109CLR can be supplied in a wide variety of packages including 2 gram (or large) BIPAX kits, pre-mixed and frozen syringes and 1 gram MINPAX. Sufficient cure is developed for polishing connectors in 20 minutes at 65°C. TRA-BOND F109CLR will complete its cure at room temperature with no pistoning.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Viscosity, After mixing
  • Hardness, Shore D
  • Adhesive Bond Strength, Lap shear, alum to alum
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, Ultimate Tg
  • Cure Time, 1 drop applications
  • Cure Time
  • Cure Time
  • Pot Life, 2 grams
  • Pot Life, 25 grams
  • Working Life, 25 grams
  • Working Life, 2 grams
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.