MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ovako S400* SB400D Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Grade SB400D is a micro-alloyed steel for general purposes with specified mechanical properties and impact requirements. The material is delivered as rolled and suitable for welding. The mechanical properties may change if the material is heat-treated. Grade SB420 is a micro-alloyed steel for general purposes with specified mechanical properties and impact requirements. The material is delivered as rolled. The mechanical properties may change if the material is heat-treated.

Information provided by Ovako

Key Words: 2142
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Flat bar
  • Hardness, Brinell, Flat bar
  • Hardness, Brinell, Flat bar
  • Tensile Strength, Flat bar
  • Tensile Strength, Flat bar
  • Tensile Strength, Flat bar
  • Tensile Strength, Yield, Rel, Flat bar
  • Tensile Strength, Yield, Rel, Flat bar
  • Tensile Strength, Yield, Rel, Flat bar
  • Elongation at Break, Flat bar
  • Elongation at Break, Flat bar
  • Elongation at Break, Flat bar
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Impact Test, Flat bar
  • Impact Test, Flat bar
  • Impact Test, Flat bar
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, Ambient temperature
  • Transformation Temperature, MS
  • Transformation Temperature, AC1
  • Transformation Temperature, AC3
  • Carbon, C
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.