MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
3M Scotch-Weld™ DP810 Tan Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel strength along with good impact resistance and durability. They can quickly bond to most metals, ceramics, rubbers, plastics and wood with minimal surface preparation.

Information provided by 3M

Vendors:
Available Properties
  • Viscosity, Accelerator
  • Viscosity, Base
  • Viscosity
  • Shear Strength, Overlap, MEK for 14 days, Cohesive Failure
  • Shear Strength, Overlap at 10 minutes after bonding
  • Shear Strength, Overlap, Acetone for 14 days, Cohesive Failure
  • Shear Strength, Overlap, Diesel Fuel for 14 days, Cohesive Failure
  • Shear Strength, Overlap, ABS, Adhesive/Cohesive Failure
  • Shear Strength, Overlap, Polycarbonate, Adhesive/Cohesive Failure
  • Shear Strength, Overlap, PVC, Substrate Failure
  • Shear Strength, Overlap, Acrylic, Substrate Failure
  • Shear Strength, Overlap, 71°C 100% RH for 14 days, Mixed Mode of AF&CF
  • Shear Strength, Overlap at 20 minutes after bonding
  • Shear Strength, Overlap, 71°C soak for 14 days, Mixed Mode of AF&CF
  • Shear Strength, Overlap at 1 hr after bonding
  • Shear Strength, Overlap, Gasoline for 14 days, Cohesive Failure
  • Shear Strength, Overlap at 2 hrs after bonding
  • Shear Strength, Overlap, Toluene for 14 days, Cohesive Failure
  • Shear Strength, Overlap at 2 hrs after bonding
  • Shear Strength, Overlap at 2 hrs after bonding
  • Shear Strength, Overlap, CRS, Cohesive Failure
  • Shear Strength, Overlap, IPA for 14 days, Cohesive Failure
  • Shear Strength, Overlap at 2 hrs after bonding
  • Shear Strength, Overlap, Stainless Steel, Cohesive Failure
  • Shear Strength, Overlap, Oily CRS, Cohesive Failure
  • Shear Strength, Overlap, 20% Bleach for 14 days, Cohesive Failure
  • Shear Strength, Overlap, 14 days, Cohesive Failure
  • Shear Strength, Overlap, Bare Aluminum, Cohesive Failure
  • Shear Strength, Overlap, Green FRP, Cohesive Failure
  • Shear Strength, Overlap, 50% Antifreeze for 14 days, Cohesive Failure
  • Shear Strength, Overlap, Abraded Aluminum, Cohesive Failure
  • Shear Strength, Overlap, Etched Aluminum, Cohesive Failure
  • Shear Strength, Overlap
  • Shear Strength, Overlap
  • Shear Strength, Overlap, Adhesion Failure
  • Shear Strength, Overlap, Cohesive Failure
  • Shear Strength, Overlap
  • Peel Strength, T-Peel
  • Cure Time, Time to Handling Strength
  • Cure Time, Full cure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.