| Wanthane® WHT-M882H is a medical grade thermoplastic polyurethane that has high hardness, high tensile strength, and high modulus. It is used in extrusion and injection applications Product ID: B22JWO4D CAS # 9018-04-06 Business Unit: Plastics Market Segments: Medical Plastic Manufacturing Process: Extrusion; Injection Applications: Medical Products Information provided by Wanhua Chemical Group Co., Ltd. |