MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Schmolz + Bickenbach Formadur® 2085 Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: FORMADUR 2085 is a free-machining corrosion-resistant mold frame steel

Characteristics: Lower mold production costs due to improved machinability; Improved corrosion resistance compared to Corroplast and Uniform hardness

Applications: Mold frames for processing corrosive plastics, Mold components and Plastic extrusion components

Heat Treatment: 1560°F- 1610°F; Cooling: Furnace 20°F/hour to 1200°F, Then air cools; Hardness: <230 HB

Information provided by Schmolz + Bickenbach

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C
  • Hardness, Rockwell C
  • Hardness, Rockwell C
  • Hardness, Rockwell C
  • Hardness, Rockwell C
  • Hardness, Rockwell C
  • Hardness, Rockwell C
  • Hardness, Rockwell C
  • Tensile Strength, Hardened and tempered to 34 HRC
  • Tensile Strength, Yield, Hardened and tempered to 34 HRC
  • Elongation at Yield, Hardened and tempered to 34 HRC
  • Reduction of Area, Hardened and tempered to 34 HRC
  • CTE, linear
  • Thermal Conductivity
  • Annealing Temperature, Soft; Hold at temperature for 30 min; Cooling: Oil; Quenched < 48 HRC
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Nickel, Ni
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.