| Solution of 1% cobalt in solvent mixture used for curing UP resins at ambient temperatures. Applications: The curing of unsaturated polyester resins at ambient temperatures can in general not be performed by an organic peroxide alone. The radical formation, which is necessary to start the polymerization reaction, is at ambient temperatures with most generally applied organic peroxides too slow. To speed up the radical formation in a controllable way organic peroxides must therefore be used in combination with a so called accelerator. For ketone peroxides like methyl ethyl ketone peroxides, cyclohexanone peroxides and acetylacetone peroxide a cobalt accelerator must be used. CAS number: 136-52-7 EINECS/ELINCS No.: 205-250-6 Information provided by Nouryon |