MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Conventus Polymers DuraPEEK XL1000 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: DURAPEEK XL1000 is a high viscosity, unreinforced, unlubricated polyether ether ketone for injection molding and extrusion and can be cross-linked after processing by heat treatment. The semi-crystalline polymer features superior property retention at elevated temperatures vs standard PEEK, while keeping same chemical resistance. This grade offers very high resistance to creep. It is a reactive system and should be processed at low melt temperatures and short cycle times.

Information provided by Conventus Polymers LLC.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break
  • Tensile Strength at Break
  • Tensile Strength at Break
  • Tensile Strength, Yield, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Strength, ASTM D790
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Strength, ASTM D695
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Compressive Modulus, ASTM D695
  • Compressive Modulus, ASTM D695
  • Shear Strength, ASTM D732
  • Shear Strength, ASTM D732
  • Shear Strength, ASTM D732
  • Coefficient of Friction, ISO 7148-2, 0.5m/s, 4N/mm2, steel
  • K (wear) Factor, ISO 7148-3, 0.5m/s, 4N/mm2, steel
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Surface Resistance, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Strength, ASTM D149
  • CTE, linear, ASTM E831, T
  • CTE, linear, ASTM E831, T>Tg, Axial
  • Glass Transition Temp, Tg, ISO 11357
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.