MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SACO AEI PEXIDAN® L/T-UV Red/White/Blue Curable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: PEXIDAN® L/T (including L/T-UV and L/T Eclipse) is a high density PEX system consisting of a silane grafted base compound A-1001 and a catalyst masterbatch CAT-003 (or A-1022 and CAT-117). When mixed and extruded in the proper proportions, the two-component system results in a material that is crosslinkable by exposure to moisture or by immersion in hot water at 90-95°C. PEXIDAN® L/T is listed by NSF International to standards 14 and 61 and to Canadian Standards Association standard B137.5. NSFI certification to ASTM F876 and ASTM F2023 testifies to its superior resistance to oxidation by hot, chlorinated water. PEXIDAN® L/T is permitted to be used in domestic continuous re-circulation systems and is listed by NSF as a NSF-pw CL5 / PEX 5006 material.

Information provided by SACO AEI Polymers.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Oxidative Induction Time (OIT), ASTM D3895
  • Melt Flow, ASTM D1238
  • Storage Temperature
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, SACO AEI DWI-QA-4007 based on ICEA T-28-562, Hot, Permanent elongation (set) after cooling
  • Elongation at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Break, SACO AEI DWI-QA-4007 based on ICEA T-28-562, Hot, Elongation under 0.2 N/mm2 load
  • Elongation at Yield, ASTM D638
  • Elongation at Yield, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Modulus, ISO 178, elastic
  • Flexural Modulus, ISO 178, elastic
  • Flexural Modulus, ISO 178, elastic
  • CTE, linear, ASTM D696
  • Specific Heat Capacity
  • Vicat Softening Point, ASTM D1525
  • Processing Temperature, barrel zones
  • Die Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.