MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metalmen Sales
Kennametal Stellite Stellite® STAR with P/M Processing
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfaces when crack free deposits are not required.

Corrosion: Corrosion resistance similar to Stellite alloy 3, but inferior to Stellite alloy 6. Excellent oxidation resistance at low temperatures, but not recommended for reducing environments. Corrosion will vary depending on concentration, temperature, stress, and type of contaminants so exposure tests are recommended.

Machinability: Stress relieve before and during machining by holding at 900°C (1650°F) for four hours and slow cool.

Wear: High tungsten content results in excellent hot hardness and low stress abrasion resistance superior to Stellite alloy 3. Wear resistance is similar to Stellite alloy 3 and is non-galling when mated with other Stellite alloys.

Data provided by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors:
Available Properties
  • Density, P/M (98%)
  • Density, Theoretical
  • Hardness, Brinell, Converted from Rockwell C hardness
  • Hardness, Brinell, Converted from Rockwell C hardness
  • Hardness, Knoop, Converted from Rockwell C hardness
  • Hardness, Knoop, Converted from Rockwell C hardness
  • Hardness, Rockwell A, Converted from Rockwell C hardness
  • Hardness, Rockwell A, Converted from Rockwell C hardness
  • Hardness, Rockwell C, Hot hardness.
  • Hardness, Rockwell C, Hot hardness.
  • Hardness, Rockwell C, Hot hardness.
  • Hardness, Rockwell C, Hot hardness.
  • Hardness, Vickers, Converted from Rockwell C hardness
  • Hardness, Vickers, Converted from Rockwell C hardness
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Elongation at Break, in 25.4 mm
  • Elongation at Break, in 25.4 mm
  • Elongation at Break, in 25.4 mm
  • Elongation at Break, in 25.4 mm
  • Modulus of Elasticity
  • Magnetic Permeability, 200 Oersted
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Melting Point
  • Solidus
  • Liquidus
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, As remainder
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Other
  • Silicon, Si
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Kennametal Stellite, former Deloro Stellite Inc

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.