MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Polikim KESTOIL® Polyamide 6 + Lubricant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combination. It is ideal for bearings without lubrication and for guides. Lubricants and impact and wear resistance increasing additives are added during production to turn Kestamid® into Kestoi®.Integrated into the material, lubricant additives become inseparable and homogenous components. Additives do not leak out even in heaviest operating conditions. Material quality and mechanical machining performance remain unaffected. No oily sensation is felt by touching the surface because additives are spread evenly inside the material.As bearing material, Kestoil® has a wear resistance 5-7 times the standard cast polyamide. This considerable result comes from the fact that the self-lubricating characteristic of the material keeps the coefficient of friction low during operation and thus prevents formation of heat between components that rub against each other. In the absence of self-lubrication, friction is reduced by external lubrication. Yet heat that is formed when lubricant is diminished or totally cleared away shortens material life due to increasing wear.Kestoil® should be preferred in applications where dimensional stability and weatherability of Kestamid® are questionable. As additives fill up pores, humidity and water absorption are reduced; sustaining dimensional stability. As the lubricant additive in Kestoil® is liquid, in high pressure and bearing applications liquid oil may leak out.

Information provided by Polikim Polimer.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Ultimate, ISO 527
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527
  • Compressive Strength, ISO 604
  • Compressive Modulus, ISO 604
  • Izod Impact, Notched (ISO), ISO 180
  • Charpy Impact Unnotched, ISO 179
  • Coefficient of Friction
  • K Factor (Wear Factor), [mg/km]
  • K (wear) Factor
  • Volume Resistivity, ISO 60093
  • Surface Resistance, ISO 60093
  • Dielectric Constant, ISO 60250
  • Dielectric Strength, ISO 50243
  • CTE, linear, ISO 11359
  • Melting Point
  • Maximum Service Temperature, Air, continuous
  • Maximum Service Temperature, Air, short term
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polikim Polimer ve Kimya Sanay

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.