MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Westlake Plastics
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Pomalux® POMC SD-A (Anti Static polyoxymethylene copolymer) is non-carbon-filled, permanently static-dissipative acetal copolymer. Surface resistivity in the 10E9 to 10E11 ohm/sq independent of humidity and temperature is typical. Natural/off white in color, this material offers enhanced lubricity, superior wear resistance, and ease of machining. Exhibiting low outgassing and non-sloughing characteristics, Pomalux® POMC SD-A is optimal for applications where sloughing cannot be accepted.

Industry: Engineering; Semiconductor and ESD

Colors Available: Black, Natural

Attributes: Optical Clarity; Transparent; Dimensional Stability; Impact Resistance

Shapes: Compression Sheet

Information provided by Westlake Plastics Co.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Surface Resistance, ASTM D257
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.