MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
DuPont Teijin Films Mylar® X842 Polyester Film, 48 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® X842 is a clear polyester film that has been chemically treated on both sides for the packaging converting market. One side is chemically treated for metal adhesion. The other side is chemically treated for print/PE extrusion.

Approvals: FDA Food Contact Status - All gauges of Mylar® X842 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers, sections (f) and (h). These regulations describe films that can safely be used in contact with all types of foods, excluding alcoholic beverages. The films listed above can be used to contain foods during oven cooking at temperatures up to and above 250°F.

Information provided by DuPont.

Vendors:
Available Properties
  • Density
  • Water Vapor Transmission, ASTM F1249, 90% RH
  • Thickness
  • Film Elongation at Break, MD, ASTM D882A
  • Film Elongation at Break, TD, ASTM D882A
  • Coefficient of Friction, Dynamic, ASTM D1894
  • Film Tensile Strength at Break, MD, ASTM D882A
  • Film Tensile Strength at Break, TD, ASTM D882A
  • Specific Heat Capacity, Typical Mylar®
  • Melting Point, Typical Mylar® via DSC
  • Maximum Service Temperature, Air
  • Shrinkage, MD, Unrestrained
  • Shrinkage, TD, Unrestrained
  • Haze, ASTM D1003
  • Transmission, Visible, ASTM D1003
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Teijin Films

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.