  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Sandvik Kanthal A Resistance Ribbon
Categories: Metal; Ferrous Metal; Ferritic; Superalloy; Iron Base

Material Notes: KANTHAL A is a ferritic FeCrAl alloy which is recommended for use at wire temperatures up to 1350°C (2460°F). In addition to industrial furnaces, it is used in appliances where its high resistivity and good oxidation resistance are of particular importance.

Typical applications for KANTHAL A are in elements embedded in ceramics for panel heaters, infrared heaters, warming plates, irons, ceramic pots, in cartridge heaters for liquid heating, storage heaters, in ceramic heaters for cooking plates, air guns, hobby kilns, radiators, in quartz tube heaters for space heating, toasters, toaster ovens, grills, industrial infrared dryers, coils on molded ceramic fibre for cooking plates with ceramic hobs.

Information provided by Sandvik

Vendors:
Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, deformation rate= 6.2x10-2/min
  • Tensile Strength, Yield
  • Elongation at Break
  • Creep Strength, 1% elongation
  • Creep Strength, 1% elongation
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus, calculated
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Curie Temperature
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Emissivity (0-1), fully oxidized
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.